Blow Moulds

Blow Moulds for Bottles, Jerrycans and Tanks That Hold an Even Wall

A blow-moulded container is only as good as its thinnest corner. We build extrusion blow moulds around the parison: the right resin, the right stretch, and a cavity that lets air do the work without thinning the part where it matters.

1–3°Draft on vertical walls
HDPE / PPMain blow resins
60–80%Tack-off mould gap rule
1.65%HDPE shrinkage, 1.5 mm wall
What we make

The parison decides the wall, not the drawing

In extrusion blow moulding, a hot tube of plastic — the parison — hangs between the mould halves, the mould closes, and compressed air expands the tube against the cooled cavity. You do not specify wall thickness directly. You specify the part weight and the minimum wall at critical points, and the parison distributes itself according to how far each area must stretch.

That is why the mould starts from the part geometry, not from a wall callout. Corners stretch the most and end up thinnest, so we use generous radii and avoid deep, narrow ribs. A parison controller can thicken the parison where the part stretches most, but the design still decides how even the wall can be.

Before tooling, we checkBlow ratio, parison weight, and neck finish.
  • Bottles, jerrycans, drums, tanks and hollow panels
  • Extrusion blow moulds, single and multi-cavity
  • Neck finishes formed by insert and blow pin
  • Handles placed where the parison can span them
Design points

Four rules that keep a blow-moulded wall even

Blow moulding fails in the geometry, not on the machine. These four rules are where it is won or lost.

Blow ratio

For a section formed between two cavity halves, keep its depth no greater than its width. Where one half forms over a core, keep the width at least twice the depth, or the wall thins to tearing.

Draft that releases

Smooth walls release with little draft because the part shrinks away from the cavity. Steps at the parting line need 10° or more, and faces formed over a core need about 5° on all sides.

Corners and radii

Corners stretch the most and end up thinnest. Generous outside radii spread the stretch, and deep narrow ribs are avoided because the parison cannot reach into them evenly.

Tack-offs that hold

Double-wall panels and cases are welded where the two walls meet. The weld holds best when the mould gap is 60–80% of the combined wall thickness, with enough space between the walls for the parison to form.

Materials

Resins for blow-moulded hollow parts

The resin sets the parison behaviour. Confirm the exact grade and melt flow index with the supplier for each order.

MaterialWhere it fitsWatch for
HDPEBottles, jerrycans, tanks, drumsHMW grade for large parts; ESC risk
PPHot-fill containers, medical bottlesHigher heat tolerance, stiffer
PETGCosmetic bottles, clear partsGlass-like clarity, high polish
PVCTechnical hollow partsCheck chemical and heat limits
Get a quote

What to send for an accurate mould quote

A complete pack lets us quote without guessing.

ItemWhat we need from you
3D modelSTEP or IGES file, plus 2D drawing
Nominal volumeTarget capacity and part weight
Resin gradeGrade, MFI, and food-contact needs
Neck finishClosure drawing and thread standard
VolumeAnnual quantity and batch size
FAQ

Questions buyers ask before tooling

Why is the wall thinner at the corners?

Because the parison stretches furthest to reach a corner, and stretching thins it. Generous radii, a shallower draw, and parison programming all help, but the geometry sets the limit.

What melt flow index suits blow moulding?

Low. Blow moulding typically needs a fractional melt flow index below 1.0 g/10 min, so the parison hangs under its own weight without stretching like taffy before the mould closes.

Can a blow mould make a hollow handle?

Yes, if the handle sits where the parison will span it when the mould closes. Its position and width affect the parison size, so handle placement is fixed before the mould is designed.

How is the neck finish formed?

The neck finish is formed by the neck insert and blow pin, then sized by trimming. Design it to the closure drawing, because the cap seals on this face.

Send the container drawing. We will check it before quoting.

Tell us the volume, the resin, and where the wall must stay thick.