Injection Molding Education
How to Design Ribs That Do Not Sink the Opposite Face
Design ribs at 50 to 60 percent of the wall thickness, and the opposite face stays flat. Add 0.5 to 1 degree of draft per side, with a small radius at the rib base. Space ribs at least twice the wall apart. A rib thicker than that rule sinks the opposite face, and no press setting removes it for good. Packing pressure can shrink the dimple, but it cannot fix a rib that is too thick. This guide gives the numbers for the drawing, the checks at T1, and the fixes when a rib must stay thick.
How do you design ribs that stay flat on the opposite face?
Keep the rib base at 50 to 60 percent of the wall it stands on.
On a 2.5 mm wall, that means a rib base of 1.25 to 1.5 mm.
On a glossy face, stay near 40 percent, since gloss shows every dimple.
The rule holds because the rib meets the wall at a junction, and that junction is thicker than either part alone.
That thick spot cools last, shrinks most, and pulls the skin on the far side inward.
The design principles guide on this site gives the same 0.5 to 0.6 range.
It caps rib height at three times the wall.
Resin changes the safe end of the range.
Semi-crystalline resins such as PP and nylon shrink more than ABS, so stay near the low end with them.
Glass-filled grades shrink less in the flow direction, but they still sink behind a rib that is too thick.
Check the resin datasheet for the shrinkage range before you freeze the rib thickness.
| Rib feature | Rule | Why it matters |
|---|---|---|
| Thickness at base | 50 to 60 percent of wall | Keeps the junction thin |
| Thickness, glossy face | Near 40 percent of wall | Gloss shows every dimple |
| Height | No more than 3 times wall | Tall ribs fill badly |
| Draft per side | 0.5 to 1 degree | Lets the rib release clean |
| Base radius | About 25 percent of wall | Cuts stress without adding mass |
| Spacing | At least 2 times wall | Lets steel between ribs cool |
Why does a thick rib sink the opposite face?
A sink mark is a shallow dimple on the face opposite a rib, a boss, or a thick section.
It forms because the thick junction cools slower than the flat wall around it.
The skin on the far side freezes first, while the core of the junction is still molten.
As that core cools, it shrinks and pulls the frozen skin inward.
The dimple sinks the opposite face exactly over the rib, so the buyer reads it as a fault in the part.
The molded part design rules on this site start from the same point.
Keep wall thickness uniform, and sink has nowhere to start.
A wall that steps from thin to thick without a taper sinks the same way.
Taper the change over a length of three times the step.
Texture hides a small sink, and polish advertises it.
That difference decides how strict the rib rule must be on each face.

How do draft and base radius change the rib?
Draft tapers the rib from base to tip, so the rib carries less mass away from the wall.
Give each side 0.5 to 1 degree, and check the draft callout on the drawing, not in a margin note.
A rib with no draft drags on the steel at ejection, and the drag shows as scuffs on the rib face.
The base radius is the second number to watch.
A sharp corner at the rib base concentrates stress, and a crack can start there in service.
A radius near 25 percent of the wall cuts that stress without adding much mass.
A radius much larger than that adds mass back at the junction, and the sink returns.
Protolabs makes the same point in its rib strength guide.
A fillet too small fails at stress, and one too large sinks again.
Keep the radius on the drawing as a number, and ask the toolmaker to hold it in steel.
How tall can a rib be, and how far apart should ribs sit?
Cap rib height at about three times the wall thickness.
A taller rib adds little stiffness, fills badly, and sticks in the tool.
Draft thins the tip of a tall rib toward nothing, so the tip can short-shot.
When one rib cannot carry the load, add a second rib instead of thickening the first.
Two thin ribs stiffen more than one thick rib, and they sink less.
Space ribs at least twice the wall apart, so the steel between them can cool.
Ribs packed tight trap heat, and the trapped heat shows as a wavy face or a sink line.
Gussets follow the same rule, since a gusset is a short rib that ties a wall to a boss.
In its uniform wall thickness guide, Protolabs puts gussets in the same 40 to 60 percent range.
When does packing fix a sink, and when does it not?
Packing pushes extra melt into the cavity after fill, and it feeds the shrinkage at the rib junction.
More packing pressure and a longer hold time shrink the dimple, but they do not remove its cause.
The gate decides how long packing can work.
A small gate freezes early, and the freeze cuts off the pack before the junction has cooled.
Plastics Technology notes the same limit in its sink reduction guide.
A tunnel gate freezes off much quicker than an edge gate, so it cuts the pack short.
Raise packing first when the sink is shallow and the rib already meets the rule.
Stop raising it when the part flashes, warps, or shows stress marks near the gate.
At that point the geometry is the fault, and the fix belongs in CAD, not on the press.
A rib at 80 percent of the wall will sink on a cosmetic face at any packing setting the press can hold.
What do you check on the drawing before steel is cut?
Read the rib thickness at the base, not at the tip, since draft thins the tip.
Check the draft on each rib face, the base radius, and the spacing between ribs.
Mark the cosmetic face on the drawing, and name the sink limit for that face in millimetres.
A rib near a side hole needs a second look.
The side hole slide guide on this site shows how a thick rib can sink the wall and shift the hole edge.
Ask the toolmaker to flag every rib above 60 percent of the wall before the DFM is signed.
Each flagged rib needs a reason in writing, or a thinner rib in its place.
Send the resin datasheet with the drawing, so the shrinkage range sits next to the rib numbers.
What should the T1 check show before you accept the part?
Hold the part at arm’s length under normal light, and look at the cosmetic face as the buyer will see it.
A sink that shows at arm’s length will show on the shelf, so it fails the cosmetic check.
Run a finger across the face behind each rib, since a dip you can feel is a dip the buyer can feel.
Measure the sink depth with a dial indicator or a depth gauge, and record it against the drawing limit.
Check every cavity, since one rib can sink in one cavity and stay flat in another.
Ask for five consecutive shots, and check the cosmetic face on each one.
Hold the texture step until the first shots pass.
The textured housing parting line guide on this site warns that texture cut too early hides sink the buyer should see first.
If the sink sits over a rib that breaks the 60 percent rule, the rib goes back to CAD.
What if the rib must stay thick for strength?
Some ribs must stay thick, because the load leaves no room for a thinner rib.
First, split the rib into two thinner ribs with a gap between them.
Second, move the rib off the cosmetic face when the part layout allows it.
Third, add texture to the face, since a grain breaks up the light and hides a shallow sink.
Fourth, gate closer to the rib so packing reaches the junction before the gate freezes.
Tooling can also help after the mold is cut, though it costs more than a CAD change.
In a GE study Plastics Technology reports, a spring-loaded boss pin cut sink by up to 50 percent on two resins.
That pin keeps pressure on the plastic under the boss as the part cools.
Gas assist and foaming can also cut sink, but they add cost and need trials of their own.
None of these fixes beats a rib sized right in CAD, so treat them as a second choice.
Mark the spacing between ribs and the cosmetic face on the same drawing.
Which rib on your part sits closest to the limit?